Molecular Formula : Zncl2
Molecular Weight : 136.29
Solidifying Proportion: 2.91
1、 Produced and tested according to the national standard GB1625-79 and department standard HG/T2323-2004.The content of Zinc Chloride ,as the main index has reached above 98%(beyond normal requirements);other indexes have reached of exceeded the normal requirements .The rate of excellent products is 100%.
2、 Throughput:10000MTS/YEAR
3、 Main use:Used as electrolyte substance of batteries ,
º Zinc Galvanizing,
º Medicine intermediates, Pesticide intermediates
º Coal washing;
º Dehydration or condensing agent in organic compound industry;
º Activator of cation exchange resin;
º Impregnant in producing PAN Polyacrylonitrile;Intermedium dyeing agent,silk luster agent,and sizing sgent in textile industry .
º Be used to produce active dyestuff and cation dyestuff.
4、 Packaging:Woven outer packaging with 2 pieces of inner plastic bags(25KGS/50KGS)
50KGS pasteboard bucket;
50KGS iron drum etc.
We can provide the highest and value services to meeting your requirements.
Technical Indexes
National Standard GB1625-79
项目Item | 指标Index |
电池级
Battery grade | 一级
First grade | 二级
Second grade |
含量(以Zncl2计)Zinc Chloride Content%≥ | 98.0 | 98.0 | 96 |
氧氯化物(以ZnO计)Hydrochloric soda content%≤ | 1.8-2.2 | 2.2 | 2.2 |
硫酸盐(以SO4计)Sulphates Content(as SO4)%≤ | 0.01 | 0.01 | 0.05 |
钡(以Ba计)% Barium Content(as Ba)%≤ | 0.1 | 0.1 | 0.2 |
铁(以Fe计)%Ferrous Content(as Fe)%≤ | 0.0005 | 0.001 | 0.002 |
铅(以Pb计)%Heavy Metal Content(as Pb)%≤ | 0.0005 | 0.001 | 0.002 |
锌片腐蚀试验zinc corrosion test | 合格Pass | - | - |
Department Standard HG/T2323-2004
项目Item | 指标Index |
Ⅰ型 | Ⅱ型 | Ⅲ型 |
优等品
Top Grade | 一等品
First grade | 优等品
Top Grade | 一等品
First grade |
含量(以Zncl2计)Zinc Chloride Content%≥ | 96.0 | 95.0 | 95.0 | 93. 0 | 40.0 |
酸水溶物 Acid Water Content%≤ | 0.01 | 0.02 | 0.05 | 0.05 | - |
氧氯化物(以znO计)Hydrochloric soda content%≤ | 2.0 | 2.0 | 2.0 | 2.0 | 0.85 |
硫酸盐(以SO4计)Sulphates Content(as SO4)%≤ | 0.01 | 0.01 | 0.01 | 0.05 | 0.0004 |
铁(以Fe计)%Ferrous Content(as Fe)%≤ | 0.0005 | 0.0005 | 0.001 | 0.003 | 0.0002 |
铅(以Pb计)%Heavy Metal Content(as Pb)%≤ | 0.0005 | 0.005 | 0.001 | 0.001 | 0.0002 |
碱和碱土含量Alkali and alkaline earth content%≤ | 1.0 | 1.0 | 1.5 | 1.5 | 0.5 |
锌片腐蚀试验zinc corrosion test | 通过Pass | - | 通过pass |